Fracture resistance of teeth restored with dentin-bonded crowns

Burke/Watts

Pages: 335-340
PMID: 7938418

While dentin-bonded crowns may hold esthetic advantages over metal-ceramic restorations, and minimal tooth preparation may also be appropriate, resistance to fracture of the restored unit is an important consideration. Dentin-bonded corwns were placed on standardized preparations in two groups of 10 maxillary premolar teeth in vitro. The preparations differed only in degree of taper. The restored specimens were subjected to compressive loading at 1 mm/min from a steel bar placed along the midline fissure. Mean fracture loads of 0.77 kN (6-degree taper) and 0.71 kN (8-degree taper) were recorded for the groups of prepared teeth, and a mean fracture load of 0.97 kN was obtained for a group of unprepared controls. Statistical analysis indicated that there was no significant difference between the fracture load of the 6-degree taper group and that of the sound control teeth.

Full Text PDF File | Order Article

 

Get Adobe Reader
Adobe Acrobat Reader is required to view PDF files. This is a free program available from the Adobe web site.
Follow the download directions on the Adobe web site to get your copy of Adobe Acrobat Reader.
  © 2014 Quintessence Publishing Co Inc
 

Home | Subscription Services | Books | Journals | Multimedia | Events | Blog
Terms of Use | Privacy Policy | About Us | Contact Us | Advertising | Help | Sitemap | Catalog