Fatigue Life of Porcelain Repair Systems

Llobell/Nicholls/Kois/Daly


PMID: 1524642

Eight intraoral porcelain repair systems, ie, Oral Ceram-Etch (Gresco), Scotchprime (3M), Rocatec (ESPE), Command Ultrafine (Kerr), Silistor (Kulzer), Clearfil Porcelain Bond (J Morita), All-Bond (Bisco), and Monobond S (Vivadent) were used in this study. The control specimens consisted of unetched porcelain surfaces onto which a resin composite was polymerized without the use of an adhesive. Load fatigue was used as the testing method to simulate the repetitive action of mastication. The peak stress applied to each test specimen was 1500 psi (10.34 MPa), and an upper limit on the number of load cycles applied to any specimen was set at 2,000,000 cycles. Statistical analysis revealed two significant subsets. Only Clearfil Porcelain Bond and All-Bond did not fail before reaching the 2,000,000-cycle upper limit.


Full Text PDF File | Order Article

 

 
Get Adobe Reader
Adobe Acrobat Reader is required to view PDF files. This is a free program available from the Adobe web site.
Follow the download directions on the Adobe web site to get your copy of Adobe Acrobat Reader.

 

© 2017 Quintessence Publishing Co, Inc

IJP Home
Current Issue
Ahead of Print
Archive
Author Guidelines
About
Accepted Manuscripts
Submission Form
Submit
Reprints
Permission
Advertising
Quintessence Home
Terms of Use
Privacy Policy
About Us
Contact Us
Help