The Effect of Finishing and Polishing on Surface Roughness of a Processed Resilient Denture Liner

Loney/Moulding


PMID: 8240651

A raised ridge on a Molloplast-B sample was removed using one of three burs, four stones, or a coarse sandpaper disc. Samples were polished using pumice alone, tin oxide alone, or both agents. A flat, unfinished sample served as a control. The average surface roughness was measured after reductions and subsequent polishings. The length of time required for initial reduction was recorded. Average surface roughness measurements ranged from 16.0 to 1.4 microns, with the control measuring 0.66 micron. Without polishing, burs produced rougher surfaces than stones and required longer times for reduction. Bur samples also remained rougher than stone samples after pumicing. No significant differences were found between treatments or controls after the use of either a combination of pumice and tin oxide or tin oxide alone.


Full Text PDF File | Order Article

 

 
Get Adobe Reader
Adobe Acrobat Reader is required to view PDF files. This is a free program available from the Adobe web site.
Follow the download directions on the Adobe web site to get your copy of Adobe Acrobat Reader.

 

© 2017 Quintessence Publishing Co, Inc

IJP Home
Current Issue
Ahead of Print
Archive
Author Guidelines
About
Accepted Manuscripts
Submission Form
Submit
Reprints
Permission
Advertising
Quintessence Home
Terms of Use
Privacy Policy
About Us
Contact Us
Help