Home Subscription Services
 
   

 
The International Journal of Prosthodontics
IJP Home Page
About the Editor
Editorial Board
Accepted Manuscripts
Submit
Author Guidelines
Submission Form
Reprints / Articles
Permissions
Advertising
MEDLINE Search
 
 
 
 
 
FacebookTwitterYouTube
Quintessence Publishing: Journals: IJP
The International Journal of Prosthodontics

Edited by George A. Zarb, BChD, DDS, MS, MS, FRCD(C)

ISSN 0893-2174

Publication:
September/October 1999
Volume 12 , Issue 5

Back
Share Abstract:

The Effects of Tooth Preparation on Pressure Measured in the Pulp Chamber: A Laboratory Study

Christopher D. J. Evans, BDSc, MDSc/Peter R. Wilson, MDS, FDSRCSEd, MS, DRDRCSEd, PhD

Pages: 439-443
PMID: 10709526

Purpose: The purpose of this study was to determine pressure changes in the pulp space during tooth preparation with either diamond or tungsten carbide burs in a high-speed dental handpiece in the laboratory. Materials and Methods: Twenty premolar teeth were collected and randomly assigned to two groups: group 1 received preparation with diamond burs and group 2 with tungsten carbide burs. The teeth were mounted on a pressure transducer and the pulp chambers were filled with saline. A 0.1-mm thickness of tooth tissue was removed from the proximal surface of each tooth, alternating dry and wet cutting, until the pulp chamber was exposed. Pressure and temperature changes were recorded during tooth preparation. Results: At 0 to 1 mm of remaining dentin depth dry cutting with diamond and tungsten carbide burs generated a mean positive pulpal pressure of 12 kPa and 6 kPa, respectively. Wet cutting under the same conditions produced 0.6 kPa and 0.15 kPa, respectively. The difference between wet and dry cutting was highly significant (P < 0.001). Diamond burs produced significantly higher pressure increases than carbide burs at all levels for both wet and dry techniques (P < 0.05). When cutting farther than 2 mm from the pulp, tooth preparation created a mean 0.09-kPa pressure increase, which was not influenced by either coolant use or bur type. The temperature change was minimal during wet cutting and only minor temperature increases were recorded during dry cutting. Conclusion: From this laboratory study it is concluded that significant pressure changes occur in the pulp chamber during tooth preparation of extracted teeth when the remaining dentin thickness is less than 2 mm.

Full Text PDF File | Order Article

 

 
Get Adobe Reader
Adobe Acrobat Reader is required to view PDF files. This is a free program available from the Adobe web site.
Follow the download directions on the Adobe web site to get your copy of Adobe Acrobat Reader.
  © 2014 Quintessence Publishing Co Inc
 

Home | Subscription Services | Books | Journals | Multimedia | Events | Blog
Terms of Use | Privacy Policy | About Us | Contact Us | Advertising | Help | Sitemap | Catalog