The effect of surface treatments on the bond strength of a nonprecious alloy-ceramic interface.

Graham JD, Johnson A, Wildgoose DG, Shareef MY, Cannavina G


PMID: 10635202

PURPOSE: The purpose of this study was to compare the effect of seven different alloy surface treatments on the bond strength of the porcelain-metal interface. MATERIALS AND METHODS: Three layers of opaque porcelain and a measured thickness of dentin porcelain were applied to nickel-chromium alloy. A tensile bond strength test was used. RESULTS: The alloy surface treatment that exhibited the highest bond strength was sandblast + surface grinding + sandblast + de-gas, whereas the alloy surface treatment that exhibited the lowest bond strength was sandblast + surface grinding + sandblast + steam cleaning + de-gas. There was a significant difference between the two methods (P < 0.05). CONCLUSION: It was concluded that de-gassing the alloy prior to porcelain application increased the bond strength and excess surface grinding of the alloy reduced bond strength; steam cleaning the alloy surface prior to de-gassing and porcelain application also significantly reduced the bond strength.


Full Text PDF File | Order Article

 

 
Get Adobe Reader
Adobe Acrobat Reader is required to view PDF files. This is a free program available from the Adobe web site.
Follow the download directions on the Adobe web site to get your copy of Adobe Acrobat Reader.

 

© 2017 Quintessence Publishing Co, Inc

IJP Home
Current Issue
Ahead of Print
Archive
Author Guidelines
About
Accepted Manuscripts
Submission Form
Submit
Reprints
Permission
Advertising
Quintessence Home
Terms of Use
Privacy Policy
About Us
Contact Us
Help