Clinical Outcome of All-Ceramic Crowns Fabricated by CAD/CAM System

K. Hikita / T. Maida / T. Fujii / T. Kawakam / T. Ishijima

Purpose: The aim of this in vivo study was to evaluate the clinical outcome of all-ceramic crowns fabricated by dental CAD/CAM GN-I (GC, Japan). Methods: A total of 125 patients were treated in 306 teeth (153 anterior teeth, 105 premolars, and 53 molars). This evaluation describes the results after a mean follow- up time of 23 months with a range from 12 to 34 months after cementation. Results: Five crowns (1 anterior tooth, 3 premolars, and 1 molar) fractured, and in all of the 5 cases the insufficient thickness of ceramic crowns was the reason for failure. Conclusion: All clinical performances of all-ceramic crowns except 5 cases were excellent. Thickness of ceramic crowns was important to prevent fracture after cementation.


Full Text PDF File | Order Article

 

 
Get Adobe Reader
Adobe Acrobat Reader is required to view PDF files. This is a free program available from the Adobe web site.
Follow the download directions on the Adobe web site to get your copy of Adobe Acrobat Reader.

 

© 2017 Quintessence Publishing Co, Inc

IJP Home
Current Issue
Ahead of Print
Archive
Author Guidelines
About
Accepted Manuscripts
Submission Form
Submit
Reprints
Permission
Advertising
Quintessence Home
Terms of Use
Privacy Policy
About Us
Contact Us
Help